MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Loxim 831 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler; Polypropylene, Flame Retardant

Material Notes:

Information provided by Loxim Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 - 1.15 g/cc1.05 - 1.15 g/ccASTM D792
Filler Content 30 %30 %
Linear Mold Shrinkage 0.011 - 0.013 cm/cm0.011 - 0.013 in/inASTM D1299
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 24.0 - 26.0 MPa3480 - 3770 psiASTM D683
Flexural Modulus 2.20 - 2.40 GPa319 - 348 ksiASTM D790
Izod Impact, Notched 0.400 - 0.600 J/cm0.749 - 1.12 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 - 115 °C230 - 239 °FASTM D1525, HDT Method B
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 30% Talc Filler
RTP Company RTP 132 HI Polypropylene (PP), High Impact - Talc
Omni Plastics OmniPro™ CPP TF30 Copolymer Polypropylene, 30% Talc reinforced
Buckeye Polymers BP RPP 3019 TU Polypropylene, 30% Mineral Filled
Buckeye Polymers BP RPP 3015 T NAT Polypropylene, Talc Filled

PLOXIM011 / 121345

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.