Colacryl® CRG107 is a hard, methyl methacrylate based, acrylic resin with exceptional pigment wetting properties. It is soluble in chlorinated hydrocarbons, ketones and lower esters and compatible with other methyl methacrylate resins and also with common plasticisers e.g. phthalates, citrates and sebacates. Applications: solid surface production and pigment dispersions Information provided by Lucite International |