MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ATG s.r.l. PVMQ Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 20 - 7020 - 70
Tensile Strength, Ultimate 6.00 - 9.00 MPa870 - 1310 psi
Elongation at Break 150 - 300 %150 - 300 %
Rebound 40 - 50 %40 - 50 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -75.0 °C-103 °F
 
Descriptive Properties
Abrasion Resistancelow
Chemical Resistance to Animal and Vegetable Oils and Greaseshigh
Chemical Resistance to Aromatic Hydrocarbonsnone
Chemical Resistance to Chloride Solventsnone
Chemical Resistance to Distilled Watermedium
Chemical Resistance to Ketoneslow
Chemical Resistance to Maximum Concentrated Alkalis (at 50°C)none
Chemical Resistance to Medium-High Concentrated Acids (at 50°C)none
Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbonslow
Compression set at 100°Chigh
Impermeability at gas (Oxygen and Nitrogen)low
Resistance to Flamemedium
Resistance to Heat Aginghigh
Resistance to Low Temperatureshigh
Resistance to Ozone and Weatheringhigh
Tear Strengthlow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATG s.r.l. NBR Nitrile-Butadiene Rubber
Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Overview of materials for Silicone Rubber
ATG s.r.l. IR Synthetic Polyisoprene
ATG s.r.l. HNBR Hydrogenated Nitrile Butadiene Rubber

PATG018 / 79383

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.