MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

3M W-610 Ceramic Microspheres
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler loadings; improve hardness; and add burnish, scrub and abrasion resistance to a variety of coating formulations. Due to the ceramic chemistry of these products, they are also UV transparent down to 250 nm and have utility in radiation-curable and thin-film powder coatings.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.50 g/cc0.0542 lb/in³
Density 2.40 g/cc0.0867 lb/in³
Particle Size 1.0 µm1.0 µm10" Percentile
 10 µm10 µm50" Percentile
 28 µm28 µm90" Percentile
 40 µm40 µm95" Percentile
pH 9.0 - 129.0 - 12ASTM E70
Specific Surface Area 3.0 m²/g3.0 m²/g
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.06.0
Compressive Strength >= 414 MPa>= 60000 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.193.19
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.30 W/m-K16.0 BTU-in/hr-ft²-°F
Softening Point 1020 °C1870 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.531.53Predominant, Becke Line
 
Descriptive Properties
ColorWhite
Oil Absorption28 gm oil/100cc microspheres
Whiteness95Hunter, "L" Value, ASTM D2244

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33035 / 167782

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.