MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Solvay RHODOLINE® 646 Surfactant
Categories: Fluid

Material Notes: Description: Highly effective mineral oil defoamer for latex processing.

Identification: OIL BASE DEFOAMER

Available in: North America

Applications: RHODOLINE© 646 may be post-added to a latex or coating color at a concentration of about 0.05 to 0.15%. For use in adhesives or paints, the suggested concentration is 2.5 to 5.0 pounds per 100 gallons of product. RHODOLINE© 646 may be stored over a wide range of temperatures. For ease of handling, storage above 40ºF is recommended. If the product should solidify due to cold, warm to room temperature and mix well before use.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 0.920 g/ccRP-17617
pH 7.0 - 9.05% Solution; RP-0420
Viscosity 200 - 750 cP#2 SP @ 30 rpm; RP-0596
Ash 10 - 12 %RP-0065
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceOpaque, Gray LiquidRP-0064
Hegman Test<6.0Grind, RP-9186

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WRHOD481 / 137712

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.