MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Spartech E65080 General Purpose PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. Best for clear tubing, profiles and hoses.

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/cc+.02
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 808010 sec ± 3
Tensile Strength, Yield 17.9 MPa2590 psi
Elongation at Break 390 %390 %
100% Modulus 9.31 MPa
@Strain 100 %
1350 psi
@Strain 100 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 °C350 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DAK Americas Laser+® MB912 PET
Colorite Polymers 2019F Rigid PVC
Axiall 6741 Moldings & Extrusions Flexible PVC
Fainplast Compounds MRT 256/G Medical Rigid PVC, Injection Molding
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber

PSPAR140 / 78762

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.