MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ 315M Clear Non-flammable, solvent based, high solids contact adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Non-flammable, solvent based, high solids contact adhesive specifically formulated for use in bonding a wide variety of materials, including decorative laminates, plywood, particleboard polyurethane foam and rigid plastics. 315M exhibits ease of sprayability, long open tack, and aggressive grab with high green strength. 315M also offers a long open time.

FEATURES: High Green Strength , Aggressive Grab Tack, High Strength Bonds, Quick Dry Time, Good Spray Pattern, Long Open Time, Excellent Adhesion to many Substrates, Flatwork Applications.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.199 g/cc
Density 9.99 lb/gal
Volatile Organic Compounds (VOC) Content 107.3 g/lPhotochemically reactive; EPA Method 24 VOC
 244.6 g/lEPA Method 24 VOC
 
Thermal PropertiesOriginal ValueComments
Boiling Point 104 - 188.6 °F
 
Descriptive Properties
Auto Ignition Temperature770 to 1033°F
ColorClear or blue
Evaporation Point<1.0
OdorMildly sweet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI912 / 232204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.