MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DAK Americas Laser+® HS AD600A PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: Laser+® HS (AD600A) is designed for PET packaging by injection stretch blow-molding using commercial heat-set technology. This polymer was formulated for processes requiring faster crystallization rates, higher glass transition and melting points, but balancing injection molding cycles speed and superior container appearance. This product is produced in Zarate, Argentina and will be supplied to customers in the Mercosur region

Application/Uses: Hot filling Bottles; Food packaging; and Packaging.

Information provided by DAK Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 51.0 lb/ft³Poured; ASTM D1895
 54.0 lb/ft³Vibrated; ASTM D1895
Particle Size 2500 µmCubical Shape
Viscosity Measurement 0.80 - 0.84VGAS-A-AN-G-V-1 (or equivalent)
 
Descriptive Properties
Color>74 CIEL*, VGAS-A-AN-G-RS-0001
 -3.1 - 0.9 CIEb*, VGAS-A-AN-G-RS-0001
 -3.3- -0.3 CIEa*, VGAS-A-AN-G-RS-0001
Compounds<2 ppmAcetaldehyde, VGAS-A-AN-G-GC-2
Fines<0.05%VGAS-A-AN-G-GA-1 (or equivalent)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced, Flame Retardant
Covestro Makroblend® UT305 PC/PET Blend
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
DAK Americas Laser+® MB912 PET
DAK Americas Laser+® HS CF746A (D53A) PET

PDAKA020 / 147995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.