MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAFAC® ASI 80 BC Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Identification: SOLUTION OF OCTYLPHOSPHONIC ACID IN DIETHYLENE GLYCOL MONOBUTYL ETHER AND WATER

CAS : 4724 – 48 – 5 and 112 – 34 – 5

Available in: Asia Pacific, Europe, Latin America and North America

Liquid above 30°C and Solid below 15°C

Solubility: Soluble in common organic solvents and partially soluble in water

Applications: Surface treatment. Pigment dispersant. Corrosion inhibitor for metalworking formulations, cleaners and industrial applications

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 2.02.05% aqueous dispersion
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 445 - 465445 - 465[mg KOH/g]; OPTI065
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 8.0 - 12 %8.0 - 12 %OPTI074
 
Descriptive Properties
Color<50Hazan, 50%, OSTMO30
Purityby 31P NMR, OPTI064>96%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Latex XZ 92229.03 Experimental Latex
Solvay RHODAFAC® H-66 E Surfactant
Solvay RHODAFAC® LO-529 Surfactant
Solvay RHODAFAC® MB Surfactant
Solvay RHODAFAC® PA32 Surfactant

WRHOD349 / 137580

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.