Notes: Elexar® EL-8431 is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar® EL-8431 is a low density, medium hardness, RoHS compliant grade suitable for both injection molding and extrusion. Features: General Purpose; Good Colorability; Good Flexibility; Halogen Free; High Elasticity; High Elongation; High Tensile Strength; Low Density; Low Flow; Low Temperature Flexibility; Low Temperature Toughness; Medium Hardness; Ozone Resistant; Sunlight Resistant (720 hours); UV Resistant; Weather Resistant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing Automotive Specifications:FORD ESB-M2D296-A Form: Pellets Processing Method: Extrusion; Injection Molding Information provided by Teknor Apex Company |