MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Engineered Syntactic Systems BZ-26 Deep Water Syntactic Foam
Categories: Polymer

Material Notes: Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high compressive and hydrostatic strengths. This yields a product able to withstand the high hydrostatic pressures experienced by today’s manned and unmanned subsea vehicles.

The BZ Grade of material is specially engineered, high performance syntactics capable of operating within much of the Bathypelagic Zone (4,000 meters or 13,100 feet). Due to the nature of the syntactic constituent materials, the BZ Grade is available in a range of densities and strengths. The product is cast in block, sheet or rod form and has isotropic properties. It may be cut or machined to any size or shape to consistent buoyancy at depth. Each block is cast as a single unit, but may be cut to fit the application requirement. Blocks or trimmed parts may also be bonded together to form a larger structure.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 24.0 - 28.0 lb/ft³
Water Absorption <= 3.0 %
@Time 86400 sec
at depth
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 3950 psi
Compressive Modulus 180 ksi
Hydrostatic Design Basis 5350 psiHydrostatic Crush Strength
 
Descriptive Properties
Service Depth (feet)9750
Service Pressure (psi)4300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
G-11 Fiberglass Epoxy Laminate Sheet
Engineered Syntactic Systems MZ-24 Deep Water Syntactic Foam
Schott BOROFLOAT® Borosilicate Float Glass
Norplex-Micarta RT342H Phenolic Cotton Laminate Tube, NEMA C
Norplex-Micarta RT342 Phenolic Cotton Laminate Tube, NEMA C

PESS954 / 93176

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.