MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SHIELD® 579 Low VOC Silver Epoxy Coating
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Description: CHO-SHIELD® 579 coating is a two component, silver-filled, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. This coating was specially developed as a variant of CHO-SHIELD® with a lower VOC rating. CHO-SHIELD® 579 dries to the touch in less than 1 hour at room temperature and attains full chemical resistance after 1 week at room temperature. However, the best electrical properties are achieved by curing at elevated temperatures.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.060 ohm-cm
@Temperature 24.0 °C,
Time 3600 sec
[ohm/sq], followed by 1 hour at 121°C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 24.0 °C
and 1 hour at 65.5°C, followed by 1 hour at 121°C
 1.00 hour
@Temperature 24.0 °C
and 1 hour at 121°C
 1.00 hour
@Temperature 24.0 °C
and 6 hours at 65.5°C
 1.00 hour
@Temperature 24.0 °C
followed by 4 hours at 79.4°C
Pot Life 480 min
Shelf Life 9.00 Month
 
Descriptive Properties
Suggested Spraying Viscosity #2 Zahn Cup18 - 24 sec
Theoretical Yield7200 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME235 / 130945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.