MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID® 6 6 GMI Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: PA 6 for injection molding, improve impact strength, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers of electric tools, automobile mirror housings, cooling screws of blowers, electromotor, bearing parts in the automotive industry. Delivered in natural color or depend to customers.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³STN EN ISO 1183-1
Linear Mold Shrinkage, Flow 0.018 cm/cm0.018 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inSTN EN ISO 294-4
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 85.0 MPa12300 psiSTN EN ISO 527-2
Elongation at Break 4.0 %4.0 %STN EN ISO 527-2
Tensile Modulus 3.20 GPa464 ksiSTN EN ISO 527-2
Flexural Strength 115 MPa16700 psiSTN EN ISO 178
Flexural Modulus 2.60 GPa377 ksiSTN EN ISO 178
Charpy Impact Unnotched 8.00 J/cm²
@Temperature -20.0 °C
38.1 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched  0.800 J/cm²
@Temperature -20.0 °C
3.81 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDSC; STN EN ISO 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FSTN EN ISO 75-2 (A)
Vicat Softening Point 215 °C419 °FB; STN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
STN EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 50.0 - 60.0 °C122 - 140 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content 0.20 %0.20 %STN EN ISO 3344
Injection Pressure 80.0 - 150 MPa11600 - 21800 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACN905 / 282497

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.