MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Zinc Nickel Alloy, UNS C73100, H06 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.69 g/cc0.314 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 180 - 210
@Load 0.500 kg
180 - 210
@Load 1.10 lb
Tensile Strength 600 - 679 MPa87000 - 98500 psi
Tensile Strength, Yield >= 579 MPa>= 84000 psi0.2% Offset
Elongation at Break >= 3.0 %>= 3.0 %
Tensile Modulus 115 GPa16700 ksi
Modulus of Rigidity 42.3 GPa6140 ksi
Poissons Ratio 0.360.36Calculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000230 ohm-cm0.0000230 ohm-cm7.5% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.9 µm/m-°C
@Temperature 20.0 - 300 °C
10.5 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 2.91 W/m-K20.2 BTU-in/hr-ft²-°F
Melting Point 1000 - 1025 °C1832 - 1877 °F
Solidus 1000 °C1832 °F
Liquidus 1025 °C1877 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 71.3 - 78 %71.3 - 78 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni 4.0 - 6.0 %4.0 - 6.0 %
Tin, Sn <= 0.10 %<= 0.10 %
Zinc, Zn 18 - 22 %18 - 22 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC73100x2 / 292496

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.