Alumina ceramic of 99.5% Al2O3 content. This material is extensively used for applications that require exceptional electrical resistance combined with resistance to chemical attack. Prime features: - Ultra-low outgassing
- Low neutron absorption
- Resistant to fluorine and chlorine attack
- Very high volume resistivity
- Good thermal conductivity
- Non-porous and vacuum tight.
Typical applications:- Gas, solid-state and waveguide lasers
- Components for a wide range of industrial, medical and defense equipment.
Information provided by Morgan Advanced Ceramics. |