MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Plyophen 43243 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: DESCRIPTION: Plyophen 43243 is a liquid one-step phenolic resin in isopropyl alcohol.

APPLICATION: Plyophen 43243 resin was developed specifically for both high and low pressure laminating processes employing glass fabrics and other inorganic reinforcing agents. This resin is capable of producing preimpregnated materials suitable for vacuum-bag molding at 10-14 psi, press molding at pressures as high as 1800 psi, or matched-metal die molding at even higher pressures. Laminates and molded parts having exceptionally high temperature resistance's are obtained with this resin.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 4.9 %Karl Fischer; DCT 4021A
pH 8.05DCT 4064A
Viscosity 460 cP
@Temperature 25.0 °C
DCT 4003F
 
Processing PropertiesOriginal ValueComments
Cure Time 180 sec
@Temperature 152 °C
DCT 5085
Gel Time 1050 min
@Temperature 135 °C
Sunshine; DCT 5091
 
Descriptive Properties
Non Volatile (%)69.5DCT 4005A-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUMIT185 / 193990

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.