MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unifrax Fiberfrax® Ball Milled Fiber High Purity Ball Milled Fiber
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These fibers can be classified into the following general categories:

  • High-Index Fibers
  • High-Temperature Fibers
  • Large-Diameter Fibers
  • Milled Fibers

Fiberfrax Milled Fibers are ball milled from Regular Fiberfrax Fibers to reduce fiber length, thus increasing the flowability and facilitating its dispersion in a matrix, such as resins or refractory cement compositions. Fiberfrax Milled Fibers can also be used as a compact filler insulation. These milled fibers can be used as a functional additive in a variety of coatings and composites to provide the following benefits:

  • Superior wear resistance
  • Improved corrosion resistance
  • Provides reinforcement and excellent compressive strength

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.73 g/cc2.73 g/cc
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1175 °C2147 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 47 - 52 %47 - 52 %
NaO2 <= 0.50 %<= 0.50 %
SiO2 48 - 53 %48 - 53 %
 
Descriptive Properties
Average Fiber Diameter (microns)1-2
ChoppingMilled
ColorWhite
Fiber Index (%)50
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CUNIF078 / 97850

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.