MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and peak molecular weight, with a slightly lower density for increased impact strength.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.947 g/ccASTM D792
Melt Index of Compound 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 3200 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 3400 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 10 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 4.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 116000 psi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 20.0 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesOriginal ValueComments
Melting Point 261 °FDow Method (DSC)
Crystallization Temperature 115 °CDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 140 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 248 °FASTM D1525
Brittleness Temperature -99.0 °FMolded and tested in accordance with ASTM D4976; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite
Bamberger Polymers Bapolene® 3295 Polyethylene, Injection Grade
Iran Petrochemical (PCC) EX7C HF4750K High Density Polyethylene
Aaron Industries AVPE HD 300-3 Virgin Polyethylene
Aaron Industries AAROLENE® ARPE HD 300-2 High Density Polyethylene Compounded Resin

PDOW1321 / 30539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.