Advantages:- Small particle size, high accumulation density, easy to blanking , easy to disperse in polymer system, etc.
- Small particle size, high accumulation density, easy to blanking , easy to disperse in polymer system, etc.
- Halogen-free flame retardant, low-toxic and low-smoke, safe and environmentally friendly, meets RoHS and REACH regulatory requirements.
Application and Suggestion:Halogen-free flame retardant FR700 can be combined with a variety of synergistic agents to achieve flame retardant requirements based on customer specific needs. In the field of thermoplastic elastomer (TPE, TPU, etc.). There are good physical properties and excellent flame retardancy in the modified system compounded with other synergists containing nitrogen or/and phosphorus.Information provided by Wynca Group |