MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type O2 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 260°C
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: Even intricate sections may be hardened, with good dimensional stability during hardening.

Key Words: UNS T31502, ASTM A681, FED QQ-T-570, SAE J437, SAE J438, DIN 1.2842, A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.61 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 624Converted from Rockwell C hardness.
Hardness, Rockwell C 55
Hardness, Vickers 602
Tensile Strength, Ultimate 1930 MPa
Tensile Strength, Yield 1750 MPa
Elongation at Break 0.00 %in 50 mm
Bulk Modulus 160 GPaTypical for steel
Shear Modulus 80.0 GPaTypical for steel
Izod Impact Unnotched 105 J
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µm/m-°C
@Temperature 25.0 - 40.0 °C
 13.0 µm/m-°C
@Temperature 25.0 - 260 °C
 14.6 µm/m-°C
@Temperature 25.0 - 540 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 260 °CTempering Temperature
 760 - 800 °CHardening Temperature
Annealing Temperature 745 - 775 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.85 - 0.95 %
Chromium, Cr <= 0.35 %
Iron, Fe 96 %As Balance
Manganese, Mn 1.6 %
Molybdenum, Mo <= 0.30 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.030 %
Vanadium, V <= 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
AISI Type O6 Tool Steel
AISI Type A2 Tool Steel
AISI Type O7 Tool Steel
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C

MSTO2 / 74495

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.