MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 11B Enriched Boron Trifluoride (High Purity Grade)
Categories: Ceramic

Material Notes: Ceradyne, Inc., a 3M company, supplies high-purity boron materials to the semiconductor market. The boron-11 isotope is used as an additive to semiconductor grade silicon as a “doping” agent, and in other semiconductor processes where ultra high purity boron is required. 3M™ 11B Enriched Boron Trifluoride is an isotopically enriched material used for doping. It is produced to >99.9% purity and >99.8% enrichment, with 25% more boron-11 than naturally occurring materials. 3M 11B enriched boron trifluoride is packaged in U.S. DOT certified cylinders. Customer cylinders may be filled upon request. Valves are CGA330 or DISS642. A minimum product order of 50 g applies.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Boron, B >= 99.8 %>= 99.8 %
 
Descriptive Properties
Impurities<15 ppmvBF3
 <15 ppmvN2
 <15 ppmvO2/Ar
 <15 ppmvCO2
 <15 ppmvSO2
 <15 ppmvHF
 <15 ppmvSiF4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM40042 / 194933

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.