MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for use with strong alkalis. Data provided by the manufacturer, Owens Corning.

Key Words: thermoset, fiber glass, fiberglass, fibreglass, fibre glass, FRP composites
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.69 g/cc0.0611 lb/in³ASTM D792
Water Absorption 0.75 %0.75 %24 hrs.; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5050
Tensile Strength, Ultimate 200 MPa29000 psiASTM D638
Modulus of Elasticity 17.0 GPa2470 ksiASTM D638
Flexural Strength 210 MPa30500 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Compressive Strength 200 MPa29000 psiASTM D695
Izod Impact, Notched 13.0 J/cm24.4 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
Dielectric Constant 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
ASTM D150
Dielectric Strength 7.87 kV/mm200 kV/inASTM D149
Arc Resistance 80 sec80 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 °C
5.00 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°F
Thermal Conductivity 0.576 W/m-K4.00 BTU-in/hr-ft²-°FASTM C177
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass
E-Polymers TEKAMID® TB110SG30 30% Glass Fiber Reinforced, High Impact PA6 Resin
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass

POC007 / 55585

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.