MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asahi Kasei Thermylene® P4-30FG-0522 PP-GF30FR
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: 30% Glass Fiber Reinforcement with Flame Retardant

Information provided by Asahi Kasei North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183A
Melt Flow 4.0 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 70.0 MPaISO 527
Flexural Strength 110 MPaISO 178
Flexural Modulus 6700 MPaISO 178
Charpy Impact, Notched 11.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 137 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436G30CL Glass Reinforced
Asahi Kasei Thermylene® P6-30FG-0600 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene
A. Schulman POLYFORT™ FPP 1239H Glass Filled Chemically Coupled Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 3459 Glass Filled Impact Copolymer
Aclo Accutech Polypropylene Homopolymer HP0339G30CL Glass Reinforced Coupled

PASAHI9906 / 220797

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.