MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

(Viewing data as-entered. Click here to return)
Magnesium Elektron Elektron® MSR-B Magnesium Casting Alloy, UNS M18220
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: ELEKTRON MSR-B is a high strength magnesium casting alloy developed by Magnesium Elektron to have good ambient and elevated temperature properties whilst retaining good foundry characteristics. It is a fully heat treatable magnesium alloy containing silver and rare earth metals. It is pressure tight, weldable and may be used up to temperatures of 200°C.

Applications: The alloys will be of interest to designers requiring good retention of properties at elevated temperatures for aerospace, automotive and military applications.

Information provided by Magnesium Elektron.

Key Words: AECMA MG-C-51; AFNOR G-Ag2.5TR; MOD DTD 5035A; UNS M18220; ISO 16220 MC65210
Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.82 g/cc
Bulk Density 0.0658 lb/in³Value supplied by MatWeb
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 80 - 105
Tensile Strength at Break >= 240 MPaMin Design Specification
 160 MPa
@Temperature 250 °C
 185 MPa
@Temperature 200 °C
 208 MPa
@Temperature 150 °C
 230 MPa
@Temperature 100 °C
 266 MPa
@Temperature 22.0 °C
Tensile Strength, Yield >= 185 MPa
@Strain 0.2 %
Min Design Specification
 122 MPa
@Strain 0.2 %,
Temperature 250 °C
 165 MPa
@Strain 0.2 %,
Temperature 200 °C
 182 MPa
@Strain 0.2 %,
Temperature 150 °C
 195 MPa
@Strain 0.2 %,
Temperature 100 °C
 205 MPa
@Strain 0.2 %,
Temperature 22.0 °C
Elongation at Break >= 2.0 %Min Design Specification
 4.0 %
@Temperature 22.0 °C
in 5.65 A½
 15 %
@Temperature 100 °C
 19 %
@Temperature 150 °C
 24 %
@Temperature 200 °C
 30 %
@Temperature 250 °C
Creep Strength 10.0 MPa
@Temperature 250 °C,
Time 3.60e+6 sec
0.1% creep
 14.0 MPa
@Temperature 250 °C,
Time 1.80e+6 sec
0.1% creep
 16.0 MPa
@Temperature 250 °C,
Time 3.60e+6 sec
0.2% creep
 21.0 MPa
@Temperature 250 °C,
Time 3.60e+6 sec
0.3% creep
 22.0 MPa
@Temperature 250 °C,
Time 1.80e+6 sec
0.2% creep
 26.0 MPa
@Temperature 250 °C,
Time 360000 sec
0.1% creep
 27.0 MPa
@Temperature 250 °C,
Time 1.80e+6 sec
0.3% creep
 34.0 MPa
@Temperature 250 °C,
Time 360000 sec
0.2% creep
 41.0 MPa
@Temperature 250 °C,
Time 360000 sec
0.3% creep
 43.0 MPa
@Temperature 250 °C,
Time 36000 sec
0.1% creep
 46.0 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
0.1% creep
 54.0 MPa
@Temperature 200 °C,
Time 1.80e+6 sec
0.1% creep
 56.0 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
0.2% creep
 65.0 MPa
@Temperature 200 °C,
Time 1.80e+6 sec
0.2% creep
 72.0 MPa
@Temperature 200 °C,
Time 3.60e+6 sec
0.3% creep
 74.0 MPa
@Temperature 200 °C,
Time 360000 sec
0.1% creep
 83.0 MPa
@Temperature 200 °C,
Time 1.80e+6 sec
0.3% creep
 86.0 MPa
@Temperature 200 °C,
Time 360000 sec
0.2% creep
 102 MPa
@Temperature 200 °C,
Time 36000 sec
0.1% creep
 103 MPa
@Temperature 200 °C,
Time 360000 sec
0.3% creep
 123 MPa
@Temperature 150 °C,
Time 3.60e+6 sec
0.2% creep
 135 MPa
@Temperature 150 °C,
Time 1.80e+6 sec
0.2% creep
 151 MPa
@Temperature 150 °C,
Time 3.60e+6 sec
0.3% creep
 160 MPa
@Temperature 150 °C,
Time 1.80e+6 sec
0.3% creep
Modulus of Elasticity 44.1 GPa
Compressive Yield Strength 165 - 200 MPa
@Strain 0.2 %
Compressive Strength 310 - 385 MPa
Poissons Ratio 0.30
Fatigue Strength 100 - 110 MPa
@# of Cycles 5.00e+7
Rotating Bend, Unnotched
Fracture Toughness 14.9 MPa-m½KIC
Shear Strength 152 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000680 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 26.7 µm/m-°C
Specific Heat Capacity 1.00 J/g-°C
Thermal Conductivity 113 W/m-K
Melting Point 550 - 640 °C
Solidus 550 °C
Liquidus 640 °C
Shrinkage 1.3 %Pattern Makers Shrinkage Factor
 
Component Elements PropertiesOriginal ValueComments
Magnesium, Mg 93 - 95.6 %As Balance
Rare Earths 2.0 - 3.0 %
Silver, Ag 2.0 - 3.0 %
Zirconium, Zr 0.40 - 1.0 %
 
Descriptive Properties
Corrosion rate430 mpyASTM B117 Salt spray test
Damping Index0.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
Magnesium Elektron Elektron® QE22 Magnesium Casting Alloy, UNS M18220
Magnesium Elektron Elektron® RZ5 Magnesium Casting Alloy, UNS M16410
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Magnesium Elektron Elektron® WE43B Magnesium Casting Alloy, UNS M18430

NMAGEL903 / 186918

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.