MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Traid Villarroya TRAIDAMID® G Nylon 6, Cast
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes:
  • High strength
  • Electrically insulating
  • Resistant to many greases, oils and fuels
  • High toughness
  • Good slide and wear resistance
Industry Applications:
  • Heavy duty industry
  • Conveyor technology
  • Textile industry
  • Engine manufacturing
  • Mechanical engineering

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
Water Absorption 0.20 %
@Time 86400 sec
DIN EN ISO 62
 0.40 %
@Time 346000 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 170 MPaISO 2039-1
Tensile Strength 83.0 MPa50 mm/min; DIN EN ISO 527-2
Tensile Strength, Yield 80.0 MPa50 mm/min; DIN EN ISO 527-2
Elongation at Break 55 %50 mm/min; DIN EN ISO 527-2
Elongation at Yield 4.0 %50 mm/min; DIN EN ISO 527-2
Modulus of Elasticity 3.50 GPa1 mm/min; DIN EN ISO 527-2
Flexural Strength 109 MPa
@Load 1.02 kg
2 mm/min; DIN EN ISO 178
Flexural Modulus 3.20 GPa
@Load 1.02 kg
2 mm/min; DIN EN ISO 178
Compressive Strength 19.0 MPa
@Strain 1 %,
Load 1.02 kg
5 mm/min; EN ISO 604
 36.0 MPa
@Strain 2 %,
Load 1.02 kg
5 mm/min; EN ISO 604
Compressive Modulus 2900 MPa
@Load 1.02 kg
5 mm/min; EN ISO 604
Charpy Impact Unnotched NBMax. 7,5j; DIN EN ISO 179-1EU
Charpy Impact, Notched 4.00 kJ/m²Max. 7,5j; DIN EN ISO 179-1EU
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+14 ohmDIN IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 23.0 - 60.0 °C
DIN EN ISO 11359-1;2
 120 µm/m-°C
@Temperature 23.0 - 100 °C
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.70 J/g-°CISO 22007-4:2008
Thermal Conductivity 0.380 W/m-KISO 22007-4:2008
Melting Point 215 °CDIN 53765
Maximum Service Temperature, Air 100 °CLong term
 170 °CShort term
Glass Transition Temp, Tg 40.0 °CDIN 53765
Flammability, UL94 HBDIN IEC 60995-11-10
 
Descriptive Properties
ColorNatural opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAID901 / 318862

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.