Hostacom CR 250 F G71412 is a 16% talc filled PP copolymer, with good UV resistance, very good impact resistance, high stiffness, good scratch resistance and improved surface appearance. Product is available as a customized color matched, pellet form. It has been designed using the latest advancements in resin synthesis and compounding technology. This grade is delivered in G71412 color version.Information provided by LyondellBasell. |