MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D1475
Viscosity 6000 cPASTM D1824
Outgassing - Total Mass Loss 0.80 %Cured property; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.020 %Cured property; at 10E-6 torr; ASTM E595
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55Cured property; ASTM D2240
Modulus of Elasticity 0.700 ksi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+14 ohm-cmCured property; ASTM D257
Insulation Resistance 1.00e+14 ohmMIL-I-46058C
Dielectric Constant 3.2
@Frequency 1000 Hz
Cured property; ASTM D150
Dielectric Strength >= 1500 V/mil
@Thickness 0.0762 mm
Cured; ASTM D149
Dissipation Factor 0.030
@Frequency 1000 Hz
Cured property; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 82.0 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 1; ASTM E831-86
 222 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 2; ASTM E831-86
Glass Transition Temp, Tg -65.0 °CCured property; ASTM E831-86
Flash Point >= 100 °CTCC
 
Descriptive Properties
ColorClear Yellow/Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound
A. Schulman BMC 850 Corrosion Resistant, Flame Retardant Molding Compound
DuPont Mobility and Materials Hytrel® HTR8136BK TPC-ET
DSM Somos® 9420 Epoxy Resin for Stereolithography
CHT Group Silcoset 101 Low Tear Condensation Cure 2-Part Molding Rubber

PAPTEK34 / 24196

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.