MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

IDI Composites E-207 Thermoset Polyester, Sheet  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: ELECTRICAL - U.L. recognized (E53587). Designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resistance. Designed to meet critical impulse and corona specifications.

Data provided by IDI Composites.

Key Words: SMC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³
Water Absorption 0.15 %0.15 %in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 39 - 4539 - 45ASTM D2583
Tensile Strength, Ultimate 124 MPa18000 psiASTM D638
Flexural Strength 234 MPa33900 psiASTM D790
Flexural Modulus 15.0 GPa2180 ksiASTM D790
Compressive Strength 234 MPa33900 psiASTM D695
Izod Impact, Notched 11.4 J/cm21.4 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 12.6 kV/mm320 kV/inASTM D149
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC
IDI Composites 46-16-60 Thermoset Polyester, Sheet
IDI Composites M-209 Thermoset Polyester, Sheet

PPTSBM / 58293

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.