MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Ateva® 2850A Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Ateva® 2850A resin is suitable for use in hot melt adhesive applications. It contains an antioxidant to minimize viscosity changes of the hot melt blends during processing. It complies with Code of Federal Regulation 21 CFR Section 177.1350 and 175.105, subject to extraction limitations for specific end use applications. Additives: Antioxidant

Applications: Adhesives & Sealants

Information provided by Celanese Corporation.

Key Words: hot melt coating and adhesive applications
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D1505; ASTM D1928 Proc A
Vinyl Acetate Content 28 %AT Plastics PTM-39
Melt Flow 850 g/10 min
@Load 0.325 kg,
Temperature 125 °C
Modified; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67ASTM D2240
Tensile Strength at Break 2.00 MPaType IV (50 mm/min); ASTM D638
Elongation at Break 550 %Type IV (50 mm/min); ASTM D638
Flexural Modulus, 1% Secant 0.00730 GPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 76.0 °CASTM E28
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Monprene® MP-2850A Thermoplastic Elastomer
Arkema EVATANE® 28-800 Copolymer Ethylene - Vinyl Acetate
Celanese Ateva® 2842A Ethylene Vinyl Acetate Copolymer
Arkema OREVAC® 9305 EVA Terpolymer
Arkema OREVAC® 9318 EVA Terpolymer

PATEVB14 / 25970

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.