MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Tipco Tipcolene® FPC 20 - 20% Calcium Carbonate Reinforced Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: 20% Calcium Carbonate Filled PP Homopolymer

Applications: General Purpose

Processing: Injection Molding

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inASTM D955
Melt Flow 9.0 g/10 min9.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 29.5 MPa4280 psiASTM D638
Elongation at Break >= 50 %>= 50 %ASTM D638
Flexural Yield Strength 43.0 MPa6240 psiASTM D790
Flexural Modulus 1.96 GPa284 ksiASTM D790
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 20% Calcium Carbonate Filled
Tipco Tipcolene® FPC 20 PPC - 20% Calcium Carbonate Reinforced Polypropylene Copolymer
Tipco Tipcolene® FPC 20 HG - 20% Calcium Carbonate Reinforced, High Gloss Polypropylene Homopolymer
Overview of materials for Polycarbonate, Molded

PTIP030 / 70248

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.