MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Alloy, UNS C12210, H10 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Spring

Fabrication Properties: Excellent Suitability - Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability - Oxyacetylene Welding, Butt Weld

Common Fabrication Processes: Blanking; Coining; Coppersmithing; Drawing; Etching; Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical Uses: Air Lines; Gasoline Lines; Hydraulic Lines; Oil Lines; Air Conditioner Tubes and Condenser Sheets; Gas Lines; Heater Lines; Heater Lines; Heather Units; Oil Burner Tubes; Air Conditioners; Refrigerators; Air Lines in Airplanes; Brewery Tubes; Casting Molds; Condenser Tubes; Dairy Tubes; Distiller Tubes; Evaporator Tubes; Gage Lines; Gasoline Lines in Airplanes; Heat Exchanger Tubes; Hydraulic Lines in Airplanes; Kettles; Oil Coolers in Airplanes; Oil Lines in Airplanes; Paper Liens; Plating Anodes; Plating Hangers; Plating Racks; Plumbing Tube; Pulp Lines; Rotating Bands; Steam Lines; Tanks; Water Lines; Oil Coolers; Oil Lines; Plumbing Fittings; Plumbing Pipe

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6262
Hardness, Rockwell F 9595
Hardness, Rockwell 30T 64
@Thickness 1.02 mm
64
@Thickness 0.0400 in
Tensile Strength 393 MPa57000 psi
Tensile Strength, Yield 365 MPa53000 psi0.2% Offset
Elongation at Break 4.0 %4.0 %
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
Forgeability 65 %65 %
Shear Strength 200 MPa29000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000326 ohm-cm0.0000326 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.9 µm/m-°C
@Temperature 20.0 - 100 °C
9.40 µin/in-°F
@Temperature 68.0 - 212 °F
 17.1 µm/m-°C
@Temperature 20.0 - 200 °C
9.50 µin/in-°F
@Temperature 68.0 - 392 °F
 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Melting Point <= 1083 °C<= 1981 °F
Liquidus 1083 °C1981 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.9 %>= 99.9 %
Phosphorus, P 0.015 - 0.025 %0.015 - 0.025 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC12210x5 / 291507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.