MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LG Chemical Lupoy 1600-03 Polycarbonate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Description: LUPOY PC 1600-03 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.

Main Characteristics: High viscosity and High melt strength

Applications: Compounds and Multi-wall sheets

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
0.32 %
@Temperature 73.4 °F
50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.00050 - 0.00070 cm/cm0.00050 - 0.00070 in/inASTM D955
Melt Flow 3.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
3.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 72.0 MPa10400 psiASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50mm/min; ASTM D638
Elongation at Break 150 %150 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.41 GPa350 ksiASTM D638
Flexural Yield Strength 96.0 MPa13900 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched 9.608 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
18.00 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
@Thickness 4.00 mm
295 °F
@Thickness 0.157 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  132 °C
@Thickness 4.00 mm
270 °F
@Thickness 0.157 in
Unannealed; ASTM D648
 143 °C
@Thickness 4.00 mm
289 °F
@Thickness 0.157 in
Annealed; ASTM D648
Vicat Softening Point 151 °C
@Load 5.10 kg
304 °F
@Load 11.2 lb
50°C/hr; ASTM D1525
Softening Point 150 - 200 °C302 - 392 °Fmelting point per MSDS
Flash Point >= 450 °C>= 842 °F
Ignition Temperature >= 450 °C>= 842 °FAutoignition
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 0.70 - 1.5 %0.70 - 1.5 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1603-03 Polycarbonate Resin
LG Chemical Lupoy 1302-05 Polycarbonate Resin
LG Chemical Lupoy 1261-03 Polycarbonate Resin
Domo TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY
Celanese Riteflex® 830 TPC, Unfilled

PLAY674 / 148684

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.