MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celcon® M50 POM, Unfilled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Celcon« M50 is a extrusion and injection molding grade with an intermediate viscosity for good processability with higher toughness than general purpose grades.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Density 1.41 g/ccISO 1183
Moisture Absorption 0.200 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.75 %ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cmASTM D955
Melt Flow 4.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
[cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 63.0 MPa50mm/min; ISO 527-2/1A
 8800 psiASTM D638
 5000 psi
@Temperature 71.1 °C
ASTM D638
 13700 psi
@Temperature -40.0 °C
ASTM D638
Elongation at Yield 12 %50mm/min; ISO 527-2/1A
Tensile Modulus 2500 MPa50mm/min; ISO 527-2/1A
Flexural Modulus 2400 MPaISO 178
 375000 psiASTM D790
 100000 psi
@Temperature 104 °C
ASTM D790
 180000 psi
@Temperature 71.1 °C
ASTM D790
Izod Impact, Notched 1.40 ft-lb/inASTM D256
 1.10 ft-lb/in
@Temperature -40.0 °C
ASTM D256
Izod Impact, Notched (ISO) 7.50 kJ/m²ISO 180/1A
Charpy Impact, Notched 8.50 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-2
Melting Point 165 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °CISO 75-1, -2
 230 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 120 °Ccavity
 180 - 200 °Chot runner
Zone 1 170 - 180 °C
Zone 2 180 - 190 °C
Zone 3 180 - 190 °C
Zone 4 190 - 200 °C
Die Temperature 190 - 200 °C
Melt Temperature 180 - 200 °C
Drying Temperature 80.0 - 100 °C
Dry Time 3.00 hour
Injection Pressure 60.0 - 120 MPa
Hold Pressure 60.0 - 120 MPa
Back Pressure <= 4.00 MPa
 
Descriptive Properties
Injection moldingYes
Injection speedslow-medium
PelletsYes
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® M90™ POM, Unfilled
Ineos H02C-00 Polypropylene Homopolymer
LyondellBasell Petrothene® LM600731X01 High Density Polyethylene, Sheet Extrusion Grade
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General
BASF Ultraform® H 2320 006 Q600 POM

PHCQ123 / 178578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.