MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex LUBMER™ TM-80B Thermoplastic Vulcanizate Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: A highly engineered thermoplastic material for use as an ultra-thin coextruded layer in demanding applications requiring, superior low friction and abrasion resistance properties. Lubmer TM-80B is a UV stable grade possessing exceptional friction and abrasion performance. TM-80B is engineered to have outstanding adhesion to Sarlink TPV materials create effective system for vehicle sealing applications such as glass run channels, waist belts, auxiliary seals, and other profiles or articles.

Availability: Europe; Asia Pacific; Latin America; North America

Features: High Stiffness; High Strength; Low Density

Uses: Bearings; Machine/Mechanical Parts

Processing Method: Injection Molding

Features: Chemical Resistant; Good Adhesion; High Hardness; High Heat Resistance; High Slip; Low Compression Set; Low Density; Low Friction; Low Specific Gravity; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ASTM D1505
Viscosity 362 cP
@Shear Rate 206 1/s,
Temperature 200 °C
362 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 66
@Time 5.00 sec
66
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 32.0 MPa4640 psiAcross Flow; ASTM D412
Elongation at Break 30 %30 %Across Flow; ASTM D412
Flexural Modulus 0.703 GPa102 ksiASTM D790
Coefficient of Friction <= 0.15<= 0.15ASTM D1894
 
Processing PropertiesMetricEnglishComments
Zone 1 177 - 210 °C350 - 410 °F
Zone 2 182 - 216 °C360 - 420 °F
Zone 3 193 - 227 °C380 - 440 °F
Zone 4 193 - 227 °C379 - 441 °F
Zone 5 193 - 227 °C380 - 440 °F
Die Temperature 193 - 227 °C380 - 440 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 6613N Impact Copolymer Polypropylene
Flint Hills P5M4R-034 Polypropylene Random Copolymer
ExxonMobil HD 6733.17 High Density Polyethylene Copolymer Resin
Eastman Piccolastic™ D125 Hydrocarbon Resin
Dow VERSIFY™ 2200 Plastomer

PTEKNQ0672 / 237163

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.