MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by Polykemi AB

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183
Melt Index of Compound 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55
@Time 15.0 sec
55
@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 19.0 MPa<= 2760 psiISO/R527
Elongation at Break 520 %520 %ISO/R527
Elongation at Yield 11 %11 %ISO/R527
Flexural Strength <= 27.0 MPa<= 3920 psiISO 178
Flexural Modulus 1.15 GPa
@Temperature 23.0 °C
167 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched  2.50 J/cm²
@Temperature -20.0 °C
11.9 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 3.40 J/cm²
@Temperature 23.0 °C
16.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °F120°C/h; ISO 75/1
Vicat Softening Point 130 °C
@Load 1.00 kg
266 °F
@Load 2.21 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °F
Injection Pressure 90.0 - 110 MPa13100 - 16000 psi
Back Pressure 0.200 - 0.500 MPa29.0 - 72.5 psi
 
Descriptive Properties
Holding Pressure20-40% of injection pressure
Injection SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYK458 / 123183

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.