MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox 29-C75 Thermoset 1,1-Di(tert-butylperoxy)-3,3,5-trimethylcyclohexane, 75% solution in isododecane
Categories: Other Engineering Material

Material Notes: Trigonox 29-C75 is a highly efficient midrange initiator (75% active ingredient in odorless mineral spirits) used for curing unsaturated polyester and vinylester resins at elevated temperatures. Typical applications include prepreg, premix, BMC, TMC, SMC and pultrusion.

CAS number: 6731-36-8

EINECS/ELINCS No: 229-782-3

Applications: Polymerization of styrene: Trigonox 29-C75 can be utilized to increase polymerization rates at temperatures between 90- 120°C (194-248°F). A comparison is made between thermally and Trigonox 29 initiated polymerization of styrene in a mass process, applying a typical temperature scheme (110-140-180°C). Due to its bifunctionality and the more constant reaction rate using Trigonox 29, the final polymer has a higher molecular weight and shows reduced dispersity. Other applications: Trigonox 29-C75 can also be used for the (co)polymerization of styrene, acrylonitrile, acrylates and methacrylates in the temperature range between 90°C and 120°C and for the polymerization of diethylene glycol di(allylcarbonate) based optical monomers. The use level of Trigonox 29-C75 will depend on the particular cure parameters being used. For Thermoset: Trigonox 29-C75 is a highly efficient midrange initiator for curing unsaturated polyester and vinyl ester resins at elevated temperatures. Typical applications include prepreg, premix, BMC, TMC, SMC and pultrusion. Trigonox 29-C75 is stable in the presence of pigments, especially carbon black, and provides excellent catalyzed shelf-life in BMC and SMC formulations.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³
Half-life  0.100
@Temperature 128 °C
0.100
@Temperature 262 °F
[hr]
 1.00
@Temperature 105 °C
1.00
@Temperature 221 °F
[hr]
 10.0
@Temperature 85.0 °C
10.0
@Temperature 185 °F
[hr]
Viscosity 9.0 cP9.0 cP
Molecular Weight 302.5 g/mol302.5 g/mol
Storage Temperature <= 25.0 °C<= 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay74.0-76.0 %
Color= 50 Pt-Co / APHA
Content0.008tert-Butyl hydroperoxide
Content (%)10.58Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1095 / 286618

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.