MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MarkeTech Lutetium Aluminum Garnet:Cerium (LAG:Ce) Scintillator Crystal  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: Lutetium Aluminum Garnet activated by Cerium is relatively dense and fast scintillation material. Its density of 6.73 g/cm3 is about 6% less than the density of BGO. Decay time is much faster (70 ns) compared to BGO (300 ns). This is advantage for time dependent and coincidence measurements.

Wavelength of scintillation emission is about 535 nm, similar as BGO (480 nm), which is ideal for Photodiode and Avalanche Diode readout. This material can by used also for Imaging Screens, similarly to YAG:Ce. The advantage of LuAG:Ce is its higher density allowing for thinner screens with higher spatial resolution. The material is mechanically and chemically stable, it can be machined to variety of shapes and sizes including prisms, spheres, and very thin plates.

Its primary advantage high density, fast decay time, a wavelength of luminescence emission well suitable for photodiode and avalanche diode readout, chemical, mechanical, and temperature resistance make it an ideal choice for PET scanners, high energy gamma and charge particle detection, and high spatial resolution Imaging Screens for Gamma, X, Beta and UV ray

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.73 g/cc
 
Descriptive Properties
Crystal StructureCubic
Luminescence: Decay Constant70 n/s
Luminescence: Photon Yield10300K; 103 pH/MeV
Luminescence: Wavelength of max emissions535 nm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Calcium Fluoride, CaF2 (Fluorite)
Harris Acoustic Sensors ELL-1203 Aluminum Substituted Narrow Line Width Garnet (3-Series)
Mateck Calcium Fluoride (CaF2)
SAES Getters Nd:YAG Solid State Laser Crystals (Nd-doped Y3Al5O12)

C5MT844 / 120753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.