MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy
Categories: Metal; Nonferrous Metal; Bismuth Alloy; Solder/Braze Alloy

Material Notes: Lowest melting point solder. Good fusible alloy used for lens blocking.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.58 g/cc0.346 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 14.5
@Load 4.00 kg
14.5
@Load 8.82 lb
2mm ball
Tensile Strength, Ultimate 41.3 MPa5990 psi
Elongation at Break 120 %120 %% elongation on 5.65 (sq. root Area) gauge length
Shear Strength 2.10 MPa305 psiShear Bond Holding Strength
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000430 ohm-cm0.0000430 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 39.8 J/g17.1 BTU/lb
CTE, linear 22.0 µm/m-°C
@Temperature 20.0 °C
12.2 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.146 J/g-°C0.0349 BTU/lb-°FSolid
 0.184 J/g-°C0.0440 BTU/lb-°FLiquid
Thermal Conductivity 18.0 W/m-K
@Temperature 85.0 °C
125 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 70.0 °C158 °FEutectic
Solidus 70.0 °C158 °F
Liquidus 70.0 °C158 °F
 
Component Elements PropertiesMetricEnglishComments
Bismuth, Bi 50 %50 %
Cadmium, Cd 10 %10 %
Lead, Pb 26.7 %26.7 %
Tin, Sn 13.3 %13.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion BrushForm® 158 Copper-Nickel-Tin Mill Hardened Strip (UNS C72900), TM00
Materion BrushForm® 158 Copper-Nickel-Tin Mill Hardened Strip (UNS C72900), TM16
AIM 47 Fusible Bismuth Alloy
Bi58-Sn42 Bismuth-Tin Eutectic Fusible Alloy
AIM 58 Fusible Alloy

NNIN06 / 18462

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.