Aeroglaze® 9741 is a two-part epoxy primer designed for use on aluminum, metal, and prepared composite surfaces. Aeroglaze 9741 primer/tie-coat is applied to scuff-sanded urethane top coats and epoxy primers. It is also used as a tie coat between scuff-sanded weather worn coatings and new urethane topcoats. Features: Meets Military Performance Requirements of Mil-P-23377. Excellent Chemical and Corrosion Resistance. Lead and Chromate-free. VOC Compliant (310 gm/liter, 2.6 lbs/gal VOC). Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016. |