MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco HDAX® SAE 30 Low Ash Gas Engine Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron HDAX Low Ash Gas Engine Oils are high quality, bright stock-free, low ash, dispersant/detergent type engine oils.

They are formulated with ISOSYN™ base stocks and an additive package containing ashless dispersant, oxidation inhibitors, metallic detergents, and a metallic antiwear agent.

Chevron HDAX Low Ash Gas Engine Oils provide outstanding oxidation and nitration resistance, which reduce the buildup of insolubles and provide extended oil and filter life. Chevron HDAX Low Ash Gas Engine Oils give excellent protection against ring and liner scuffing and wear. They also minimize valve recession in four-stroke engines and provide excellent piston and ring belt deposit control and effectively protect against the formation and buildup of engine sludge.

Applications

Chevron HDAX Low Ash Gas Engine Oils are especially formulated to meet API CD performance and Engelhards NSCR catalyst compatibility requirements.

Chevron HDAX Low Ash Gas Engine Oils are recommended for four-cycle and selected two-cycle stationary engines fueled by natural or synthetic gas and gas from digester and landfill sources. These oils are recommended for four-cycle engines manufactured by Caterpillar, Delaval-Enterprise, Dresser-Rand Categories I, II and III (SAE 30), Fairbanks-Morse/MEP, Superior, Waukesha, and Worthington. They are also satisfactory for selected two-cycle engines manufactured by Clark-Dresser and Worthington.

Key Words: CPS Number: 232327; MSDS Number: 7046
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29.8 °
Viscosity Measurement 104Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 97.3 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 11.4 cStASTM D445
Ash 0.50 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 4.2ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -24.0 °CASTM D97
Flash Point 222 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.027 %
Zinc, Zn 0.032 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Regular Unleaded Gasoline
ChevronTexaco Supreme Unleaded Gasoline
ChevronTexaco Plus Unleaded Gasoline
ChevronTexaco HDAX® SAE 30 Ashless Gas Engine Oil
ChevronTexaco HPLX SAE 30 Chevron HPLX Low Ash Gas Engine Oil

WCHEV061 / 74676

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.