FRAGOM: is the trade-mark of our flame retardant halogen free polyolefine compounds. FRAGOM G/2000 1: flame retardant crosslinkable compound having GOOD RESISTANCE TO OIL and DIESEL for insulation and sheathing. It is a conveniently grafted compound able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/100 SCU. REACTION BETW EEN GRAFTING AND CATALYST These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5 Certify: GOST 305 Information provided by Crosspolimeri S.P.A. |