MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® 63H NT0752 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Vydyne 63H NT0752 is a medium-viscosity, heat stabilized PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. 63H NT0752 resin offers high strength, rigidity, and toughness over a broad range of demanding applications, good fluid resistance to a wide variety of chemicals, solvents and oils, and heat stability to ensure property longevity when the material is subjected to higher temperatures.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 2.5 %2.5 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 8.5 %8.5 %ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cm
@Thickness 2.00 mm
0.019 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm
@Thickness 2.00 mm
0.019 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiDAM; ISO 527-2
 65.0 MPa9430 psi50% RH; ISO 527-2
Tensile Strength, Yield 55.0 MPa7980 psi50% RH; ISO 527-2
 85.0 MPa12300 psiDAM; ISO 527-2
Elongation at Break 25 %25 %DAM; ISO 527-2
 200 %200 %50% RH; ISO 527-2
Elongation at Yield 5.0 %5.0 %DAM; ISO 527-2
 20 %20 %50% RH; ISO 527-2
Tensile Modulus 1.70 GPa247 ksi50% RH; ISO 527-2
 3.20 GPa464 ksiDAM; ISO 527-2
Flexural Strength 20.0 MPa2900 psi50% RH; ISO 178
 70.0 MPa10200 psiDAM; ISO 178
Flexural Modulus 0.700 GPa102 ksi50% RH; ISO 178
 2.50 GPa363 ksiDAM; ISO 178
Poissons Ratio 0.400.40ISO 527-2
Izod Impact, Notched (ISO)  5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 25.0 kJ/m²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 250 - 295 °C482 - 563 °FExtrusion
Zone 2 250 - 295 °C482 - 563 °FExtrusion
Zone 3 250 - 295 °C482 - 563 °FExtrusion
Zone 4 250 - 295 °C482 - 563 °FExtrusion
Zone 5 250 - 295 °C482 - 563 °FExtrusion
Die Temperature 270 - 295 °C518 - 563 °FExtrusion
Melt Temperature 270 - 295 °C518 - 563 °FExtrusion
 
Descriptive Properties
AdditiveHeat Stabilizer
Agency RatingsASTM, D4066 PA0122
 ASTM, D6779 PA0122
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
AppearanceNatural Color
FeaturesChemical Resistant
 General Purpose
 Good Toughness
 Heat Stabilized
 High Melt Strength
 High Rigidity
 High Strength
 Medium Viscosity
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodOther Extrusion
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9236 / 287593

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.