MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate
Categories: Ceramic; Oxide; Silicon Oxide; Zirconium Oxide; Potting/Casting Ceramic

Material Notes: Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing.

Cure:
Step 1. Dry for 8 hours minimum at room temperature.
Step 2. Bake at 200 ºF for 2–4 hours.
Step 3. Final cure at 250 ºF for 3 hours.
Step 4. Final cure at 450 ºF for 30–60 minutes if using HLB-1 Hydrophobic Liquid Binder.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 105 lb/ft³Powder
Porosity <= 2.0 %
pH 2.0 - 3.0
Viscosity 15000 cP
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 8000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cm
Dielectric Strength 125 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.70 µin/in-°F
@Temperature 20.0 °C
Maximum Service Temperature, Air 2800 °F
Shrinkage <= 0.30 %
@Temperature 538 °C
 
Processing PropertiesOriginal ValueComments
Dry Time >= 8 hourAir dry
Cure Time 5.00 - 7.00 hour2-4 hrs at 200°F; 3 hrs at 250°F
Pot Life 60 - 120 min
Shelf Life 12.0 Month
 
Descriptive Properties
Acid ResistanceGood
Alkali ResistanceGood
BinderMgO-P2O5
ColorOff White
Mix Ratio100:13-15
Moisture ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina
Aremco Ceramacast™ 673-N High Temperature Potting & Casting Material Silicon Carbide
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate

CAREM46 / 587

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.