MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Formosa Plastics TAIRILAC® AG10AP ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Product Description: Extrusion Grade. Characteristics: Extrusion molding; Super High impact; High rigid.
Availability: Asia Pacific; Europe; North America
Features: High Rigidity; Ultra High Impact Resistance
Agency Rating: EC 1907/2006 (REACH)
RoHS Compliance: RoHS Compliant
UL File Number: E162823
Processing Method: Extrusion

Information provided by Formosa Chemicals & Fiber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 in/in
@Thickness 3.20 mm
ASTM D955
Melt Flow 4.6 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 93ASTM D785
Tensile Strength 5510 psiASTM D638
Flexural Modulus 270000 psiASTM D790
Izod Impact, Unnotched 9.00 ft-lb/in
@Thickness 6.35 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 183 °FUnannealed, 1/4" bar; ASTM D648
 201 °F
@Temperature 80.0 °C,
Time 28800 sec
Annealed; ASTM D648
Vicat Softening Point 212 °F
@Load 1.02 kg
ASTM D1525
Flammability, UL94 HB
@Thickness 1.52 mm
All Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFPCPD011 / 268125

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.