Description: Highly effective mineral oil defoamer for latex processing. Identification: OIL BASE DEFOAMER Available in: North America Applications: RHODOLINE© 679 is recommended for application at 0.1 – 0.5% to provide good foam control. For best results, RHODOLINE© 679 should be added directly to the system. Information provided by Rhodia, Rhodia has been acquired by Solvay. |