Physical Properties | Metric | English | Comments |
---|
Density | 1.469 g/cc @Temperature 100 °C | 0.05307 lb/in³ @Temperature 212 °F |
| 1.475 g/cc @Temperature 90.0 °C | 0.05329 lb/in³ @Temperature 194 °F |
| 1.482 g/cc @Temperature 80.0 °C | 0.05354 lb/in³ @Temperature 176 °F |
| 1.489 g/cc @Temperature 70.0 °C | 0.05379 lb/in³ @Temperature 158 °F |
| 1.496 g/cc @Temperature 60.0 °C | 0.05405 lb/in³ @Temperature 140 °F |
| 1.503 g/cc @Temperature 50.0 °C | 0.05430 lb/in³ @Temperature 122 °F |
| 1.51 g/cc @Temperature 40.0 °C | 0.0546 lb/in³ @Temperature 104 °F |
| 1.518 g/cc @Temperature 30.0 °C | 0.05484 lb/in³ @Temperature 86.0 °F |
| 1.525 g/cc @Temperature 20.0 °C | 0.05509 lb/in³ @Temperature 68.0 °F |
| 1.532 g/cc @Temperature 10.0 °C | 0.05535 lb/in³ @Temperature 50.0 °F |
| 1.54 g/cc @Temperature 0.000 °C | 0.0556 lb/in³ @Temperature 32.0 °F |
Viscosity | 3.41 cP @Temperature 100 °C | 3.41 cP @Temperature 212 °F |
| 4.36 cP @Temperature 90.0 °C | 4.36 cP @Temperature 194 °F |
| 5.6 cP @Temperature 80.0 °C | 5.6 cP @Temperature 176 °F |
| 7.6 cP @Temperature 70.0 °C | 7.6 cP @Temperature 158 °F |
| 10.4 cP @Temperature 60.0 °C | 10.4 cP @Temperature 140 °F |
| 15.8 cP @Temperature 50.0 °C | 15.8 cP @Temperature 122 °F |
| 25.5 cP @Temperature 40.0 °C | 25.5 cP @Temperature 104 °F |
| 47.7 cP @Temperature 30.0 °C | 47.7 cP @Temperature 86.0 °F |
| 120 cP @Temperature 20.0 °C | 120 cP @Temperature 68.0 °F |
Molecular Weight | 40.01 g/mol | 40.01 g/mol |
|
Thermal Properties | Metric | English | Comments |
---|
Specific Heat Capacity | 2.93 J/g-°C @Temperature 150 °C | 0.700 BTU/lb-°F @Temperature 302 °F |
| 2.96 J/g-°C @Temperature 100 °C | 0.707 BTU/lb-°F @Temperature 212 °F |
| 3.01 J/g-°C @Temperature 100 °C | 0.719 BTU/lb-°F @Temperature 212 °F |
| 3.016 J/g-°C @Temperature 30.0 °C | 0.7208 BTU/lb-°F @Temperature 86.0 °F |
| 3.04 J/g-°C @Temperature 150 °C | 0.727 BTU/lb-°F @Temperature 302 °F |
| 3.06 J/g-°C @Temperature 30.0 °C | 0.731 BTU/lb-°F @Temperature 86.0 °F |
| 3.07 J/g-°C @Temperature 100 °C | 0.734 BTU/lb-°F @Temperature 212 °F |
| 3.11 J/g-°C @Temperature 150 °C | 0.743 BTU/lb-°F @Temperature 302 °F |
| 3.12 J/g-°C @Temperature 30.0 °C | 0.746 BTU/lb-°F @Temperature 86.0 °F |
| 3.13 J/g-°C @Temperature 100 °C | 0.748 BTU/lb-°F @Temperature 212 °F |
| 3.16 J/g-°C @Temperature 50.0 °C | 0.755 BTU/lb-°F @Temperature 122 °F |
| 3.18 J/g-°C @Temperature 150 °C | 0.760 BTU/lb-°F @Temperature 302 °F |
| 3.18 J/g-°C @Temperature 20.0 °C | 0.760 BTU/lb-°F @Temperature 68.0 °F |
| 3.19 J/g-°C @Temperature 100 °C | 0.762 BTU/lb-°F @Temperature 212 °F |
| 3.21 J/g-°C @Temperature 50.0 °C | 0.767 BTU/lb-°F @Temperature 122 °F |
| 3.23 J/g-°C @Temperature 20.0 °C | 0.772 BTU/lb-°F @Temperature 68.0 °F |
| 3.98 J/g-°C @Temperature 150 °C | 0.951 BTU/lb-°F @Temperature 302 °F |
Boiling Point | 142.5 °C | 288.5 °F |
| 150.1 °C | 302.2 °F |
|
Descriptive Properties |
---|
Color | colorless |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.