MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro HYPERLITE® E-855 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Hyperlite E-855 is a polymer polyol, which is used in a broad range of urethane foam and other applications.

Properties / Applications: Hyperlite E-855 is a polymer polyol, which is used in a broad range of urethane foam and other applications. It is especially suited for rapid-demold high-resiliency (HR) foam, and is typically used in molded urethane foam for automotive seat cushions and backs, as well as interior trim components. The Hyperlite E-855 polymer polyol, when blended with Hyperlite polyether polyols, produces foams with inherent stability during molding, excellent breathability characteristics, and a high level of strength, durability, and load-bearing properties. As with any product, the use of Hyperlite E-855 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Bulk Density 65.8 lb/ft³
Molecular Weight 96800 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point 213 °CPMCC
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.060 %
 
Descriptive Properties
AppearanceWhite, viscous liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0793 / 202576

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.