MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Fortron® 6850 L6 Polyphenylene Sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: Low warp, excellent flow properties

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccASTM D792
Water Absorption 0.020 %ASTM D570
Linear Mold Shrinkage, Flow 0.0025 cm/cm
Linear Mold Shrinkage, Transverse 0.0035 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 96ASTM D785
Tensile Strength, Ultimate 124 MPaASTM D638
Elongation at Break 1.0 %ASTM D638
Flexural Strength 193 MPaASTM D790
Flexural Modulus 16.5 GPaASTM D790
Izod Impact, Notched 0.400 J/cmASTM D256
Izod Impact, Unnotched 2.70 J/cmASTM D4812
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Strength 11.0 kV/mm
@Thickness 3.17 mm
ASTM D149
Dissipation Factor 0.00090
@Frequency 1e+6 Hz
ASTM D150
 0.0010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
CTE, linear, Transverse to Flow 17.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 280 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °CASTM D648
UL RTI, Electrical 220 °C
UL RTI, Mechanical without Impact 220 °C
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Fortron® 4184 L4 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Celanese Fortron® 6165 A4 Polyphenylene Sulfide (PPS), 65% Mineral/Glass-Fiber
Celanese FORTRON® 9205C4 Polyphenylene Sulfide (PPS)
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS)
Celanese Fortron® 1140 L4 Polyphenylene Sulfide (PPS), 40% Glass Fiber

PHCU27 / 45767

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.