MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Rilsamid® MA 4411 NAT PA12-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 235 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength, Yield 25.0 MPaCond.; ISO 527-1/-2
Elongation at Break >= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 23 %Cond.; ISO 527-1/-2
Tensile Modulus 470 MPaCond.; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 175 °C10°C/min; Dry; ISO 11357-1/-3
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
PlasticizerYes
Processing MethodsOther Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsamid® AMVO TLD PA12
Arkema Rilsamid® MA 4411 BLACK PA12-I
Arkema Rilsan® BECNO TL PA11
Arkema Rilsan® Tieflex R463 NAT TL PA
Arkema Rilsamid® AMN BLACK P40 TLD PA12

PARKF876 / 193624

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.