MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Polymer Technology & Services, LLC (PTS)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.15 %24 hours at 73°F
Melt Flow 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 60.3 MPa
@Thickness 3.17 mm
Elongation at Break 100 %
@Thickness 3.17 mm
Flexural Yield Strength 89.6 MPa
@Thickness 3.17 mm
Flexural Modulus 2.21 GPa
@Thickness 3.17 mm
Izod Impact, Notched 6.94 J/cm
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °CASTM D648
Flammability, UL94 V-2
@Thickness 1.59 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Clear grade, but transmission not quantified.
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 470 - 500 °F
Middle Barrel Temperature 480 - 500 °F
Front Barrel Temperature 500 - 520 °F
Nozzle Temperature 490 - 520 °F
Melt Temperature 500 - 540 °F
Mold Temperature 160 - 200 °F
Drying Temperature 250 °F
Dry Time 3 - 4 hour
Injection Pressure 7500 - 18000 psi
Back Pressure 50.0 - 200 psi
Clamp Pressure 4000 - 10000 psi
Cycle Time - Injection 1.0 - 2.5 sec
Cycle Time - Cooling 5.0 - 40 sec
Vent Depth 0.00200 - 0.00800 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Injection Speed- Edge GateSlow-Medium
Injection Speed- Tab GateMedium-Fast
Injection Speed- Tunnel GateFast
Shot Size40-60%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Samyang Trirex® 3020U UV Stable Polycarbonate
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate
Chi Mei Polylac® PA-717 General Purpose ABS Resin
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release

PLBS08 / 50462

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.